Elastomer / Flexible Industrial Grade
PEBA

PEBA – Polyether Block Amide for Sustained Flexing and Cold

An elastomer with over 1000 % elongation at break and 36 MPa strength (ASTM D638) at 1.0 g/cm³. Impact test at −40 °C without break.

Technical Specifications

Base Polymer
Polyether block amide (PEBA), Shore 42D
Shore Hardness
Shore 42D
Tensile Strength
36 MPa at break (ASTM D638)
Heat Deflection
no HDT/Vicat in the datasheet; impact test at −40 °C without break (ASTM D256)
UV Resistance
Not UV-stabilized

Typical Applications

  • Dynamically loaded spring and hinge elements
  • Parts for cold environments – impact test at −40 °C without break
  • Bellows and boots with high elongation
  • Lightweight elastomer parts – density 1.0 g/cm³
  • Buffers and grips with high tear strength

Compliance Evidence

RoHS

Free of hazardous substances (lead, mercury, cadmium, hexavalent chromium, PBB, PBDE) per EU Directive 2011/65/EU. Safe for commercial use in the EU.

Evidence: Manufacturer declaration for the filament: does not contain the restricted substances. Applies to the filament, not to the printed part.

REACH

Compliant with the EU chemicals regulation REACH (EC) No. 1907/2006. Contains no SVHC substances (Substances of Very High Concern) above threshold values.

Evidence: Manufacturer declaration: manufactured in compliance with RoHS and REACH. Applies to the filament, not to the printed part.

Material Documents

Technical Datasheet

Official manufacturer source · PDF

Safety Data Sheet

Official manufacturer source · PDF

Compliance Certificate

Official manufacturer source · PDF

PEBA filament spool

Material profile

PEBA stands for polyether block amide: a block copolymer alternating hard polyamide segments with soft polyether segments. The hard blocks carry the load, the soft ones allow the elongation. The result is an elastomer that deforms a long way, takes comparatively high stress while doing so, and at 1.0 g/cm³ is lighter than any TPU.

In industry the material has been at home for decades wherever parts go through thousands of load cycles. As a filament it is a niche – and accordingly has few, but meaningful, datasheets.

Documented figures

The following values come from the manufacturer datasheet for Fillamentum Flexfill PEBA 90A. It is the datasheet in this class with the broadest test basis – including abrasion, tear strength and two test temperatures in the impact test.

PropertyValueStandard
Hardness42 Shore DASTM D2240
Strength at break36 MPaASTM D638
Stress at 50 % elongation9 MPaASTM D638
Elongation at break> 1000 %ASTM D638
Flexural modulus65 MPaASTM D790
Izod impact, notched, 23 °Cno breakASTM D256
Izod impact, notched, −40 °Cno breakASTM D256
Tear strength, unnotched115 kN/mISO 34-1
Tear strength, notched85 kN/mISO 34-1
Abrasion loss< 48 mm³ (10 N / 40 m)ISO 4649
Density1.0 g/cm³ISO 1183

For context: the product name carries the designation “90A”, while the figure measured and reported in the datasheet is 42 Shore D to ASTM D2240. Shore A and Shore D are different test scales – 42 D sits roughly in the 90 A region, but it is the actually tested value, so that is what we state.

What separates PEBA from TPU

PEBATPU 95AFoamed TPU
Elongation at break> 1000 %grade-dependent475–629 %
Density1.0 g/cm³~1.1–1.2 g/cm³0.51–0.88 g/cm³ (part)
Coldimpact at −40 °C without breaknot documentednot documented
Oil contactnot documenteddocumented good resistancedocumented good resistance
Heat deflectionnot documented~70–80 °CVicat 53–83 °C

PEBA plays to its strengths in elongation, weight and cold. Where media contact dominates – oils, greases, cutting fluid – TPU remains the better documented choice.

Design notes

  • Plan for elongation, not stiffness. At 65 MPa flexural modulus PEBA is not a dimensionally stiff part. Where a contour has to hold, it needs a rigid counter-structure.
  • Separate the load path. Bolted joints run through inserts, threaded inserts or a rigid plate – not through the elastomer.
  • Print slowly. 20 to 40 mm/s, bed 70 to 90 °C, heated chamber recommended by the manufacturer. The material is dried before printing.
  • Do not assume a thermal rating. With no HDT or Vicat figure in the datasheet there is no defensible service temperature. Where it gets warm, the case has to be checked beforehand.

What is not documented

PEBA is frequently advertised with four properties that are backed by a test standard in no manufacturer document we checked – not even in the raw material datasheet of the pellet producer:

  • Rebound resilience (“energy rebound”) – no measured value, no standard, in any document.
  • Flex fatigue / dynamic endurance – no De Mattia, Ross-Flex or comparable test.
  • UV and weather resistance – no figure with a test standard.
  • Heat deflection (HDT/Vicat) – not stated for any of the PEBA filaments we checked.

We do not put such properties on a datasheet while they are undocumented. If your part depends on one of them, that is a case for testing on the actual component – talk to us before you design around it.