High Performance Industrial Grade
PPS-GF

PPS-GF – Glass fiber PPS for 236 °C

PPS-GF: 20 % glass fiber, HDT/A 236 °C annealed, UL94 V-0, 6.05 kV/mm dielectric strength. An insulating high-temperature material.

Technical Specifications

Base Polymer
Polyphenylene sulfide with 20 % short glass fiber (GF)
Tensile Strength
64.1 MPa (X-Y, ISO 527)
Heat Deflection
236.3 °C (HDT/A, annealed)
UV Resistance
Not UV-stabilized

Typical Applications

  • High-voltage and RF insulation in industry and automotive
  • Parts in continuous use above 200 °C
  • Chemically loaded parts with a flame retardancy requirement
  • Test and soldering fixtures in electronics manufacturing

Compliance Evidence

UL

Flammability rating per UL test standard. Applies to the tested filament under defined conditions.

Note: UL94 V-0 at 1.5 mm per the manufacturer datasheet (filament, not automatically the printed part).

UL ratings in 3D printing apply only to the specifically tested combination of material, printer, nozzle, layer height and profile. UL evidence from other process combinations does not transfer to this service.

Documents will be provided once a specific material is selected.

Material profile

PPS-GF is polyphenylene sulfide with 20 % short glass fiber and the most demanding material in the portfolio. The combination of 236 °C heat deflection, a documented V-0 class and 6.05 kV/mm dielectric strength does not exist anywhere else in FFF printing.

The difference from the PPS-CF already on offer is electrical. Carbon fiber conducts, glass fiber insulates. For high-voltage components, RF assemblies and anything sitting near live parts, that is not a convenience feature but a prerequisite.

Values from the manufacturer datasheet

PropertyX-YZTest standard
Tensile strength64.1 MPa22.9 MPaISO 527
Tensile modulus4,552 MPa2,557 MPaISO 527
Elongation at break2.0 %1.1 %ISO 527
Flexural strength102.3 MPa45.7 MPaISO 178
Flexural modulus4,111 MPa2,606 MPaISO 178
Charpy notched7.3 kJ/m²ISO 179
HDT (1.8 MPa)125.8 °CISO 75
HDT/A (0.45 MPa)236.3 °CISO 75
Vicat272.5 °CISO 306
Decomposition440.2 °CTGA
Flame classV-0 at 1.5 mmUL 94
Dielectric strength6.05 kV/mmIEC 60243-1
Dielectric constant (1 MHz)2.71IEC 60243-1
Water absorption0.11 %—
Density1.36 g/cm³ISO 1183

All HDT values apply to specimens annealed for 10 hours at 130 °C.

Processing

Nozzle 310–350 °C, bed 80–90 °C, fan off, print speed up to 250 mm/s. Drying 10 hours at 100 °C, storage below 20 % relative humidity. Annealing follows printing – without it, heat deflection stays far below the datasheet figure. A hardened nozzle from 0.4 mm is mandatory.

Request a Quote